The results in this letter show the possibility of realizing a high magnetoelectric (ME) coefficient material by synthesizing the particulate composites of ferroelectric and ferromagnetic components using the annealing and aging treatment. The ME composites were fabricated using a combination of conventional mixed oxide sintering and thermal treatment. The thermal treatment constituted of annealing at temperature closer to calcination temperature (∼800°C) followed by aging at lower temperatures (300–400°C). Microstructure of the fabricated samples was analyzed using the X-ray mapping in scanning electron microscopy (SEM) and it was found that NiFe 1.9 Mn 0.1 O 4 (NFM) is distributed inside the Pb(Zr 0.52 Ti 0.48 )O 3 (PZT) grains on the length scales of 100 nm. The magnitude of piezoelectric constant ( d 33 ) and the dielectric constant exhibited significant variation with aging time and temperature. It was found that the magnitude of ME coefficient for PZT–5NFM sample increased from 37 to 56 mV/cm·Oe after thermal treatment, an enhancement of ∼50%.
No takes yet. Share an insight, caveat, or question.
Islam et al. (2006) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: