The pitting corrosion behaviors between the constituent phases in F53 super duplex stainless steel (SDSS) in acidified chloride environments were investigated using a critical pitting corrosion temperature test, a potentiodynamic anodic polarization test, and the microstructure analyses through a SEM-EDS and a SAM. As the solution annealing temperature decreased from <TEX>1150∘C</TEX> to <TEX>1050∘C</TEX>, the <TEX>γ</TEX>-phase fraction increased whereas the <TEX>α</TEX>-phase fraction decreased. The pitting potential and the critical pitting temperature increased with a decrease of solution annealing temperature, thereby increasing the resistance to pitting corrosion. The pitting corrosion of the SDSS was selectively initiated at the <TEX>α</TEX>-phases because the PREN (pitting resistance equivalent number, PREN = %Cr+3.3%Mo+30%N) value of the <TEX>γ</TEX>-phase is much larger than that of the <TEX>α</TEX>-phase, irrespective of the solution annealing temperature. The pitting corrosion was finally propagated from the <TEX>α</TEX>-phase to the <TEX>γ</TEX>-phase. The decrease of solution annealing temperature enhanced the resistance to pitting corrosion greatly in acidified chloride environments due to a decrease of PREN difference between the <TEX>γ</TEX>-phase and the <TEX>α</TEX>-phase, that is, a decrease of <TEX>PRENγ</TEX> by dilution of N in <TEX>γ</TEX>-phase with an increase in the <TEX>γ</TEX>-phase volume fraction and an increase of <TEX>PRENα</TEX> by enrichment of Cr and Mo in the <TEX>α</TEX>-phase with a decrease in the <TEX>α</TEX>-phase volume fraction.
No takes yet. Share an insight, caveat, or question.
Kim et al. (2014) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: