Answers are grounded in this paper and cite their sources.
Deposition Technique using Ammonia (NH 3 ) as a complexing agent. Thin films of ZnO are deposited onto glass substrates at room temperature for 5hours. The optical properties of the films were measured using Double Beam UV-Spectrophotometer with serial number UV061514, Rutherford Back Scattering Spectroscopy (RBS) analysis revealed that the thin filmshave percentage ratios of the elements of Zn/O, 47/53 as annealed for 3hours at the temperature of 250C and Zn/O, 48.8/51.2as annealed for 1hour at the temperature of 150C. The thicknesses are 80nm for 3hours and 150nm for 1hour asannealed samples at 250C and 150C respectively. It was found that ZnO thin films exhibits n-type conduction. Optical band gap values of the twosamples are 3.10.05eV as annealed for 3hours and 3.30.05eV as annealed for 1hour with an average of 3.20.05eV. Other optical properties calculated from transmittance using appropriate equations are absorbance, reflectance, band gap , absorption coefficient, optical conductivity, refractive index and extinction coefficient.
No takes yet. Share an insight, caveat, or question.
Onwuemeka et al. (2014) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: