In this research, WS 2 nanoparticles were synthesized using hydrothermal method then added to aluminum matrix as reinforcement. Nanocomposites were fabricated by powder metallurgy processing followed by Spark Plasma Sintering (SPS) consolidation. Microstructural, mechanical, and tribological properties of nanocomposites were investigated using optical microscopy (OM), field emission scanning electron microscopy (FESEM), energy dispersive spectroscopy (EDS), uniaxial compression test and ball on disc tribometer. Microscopic analyses confirm the formation of well homogenized Al-WS 2 nanocomposites. Mechanical evaluations indicate that, the increase in weight fraction of WS 2 nanoparticles, results in improvement of hardness and compressive strength of aluminum. Addition of WS 2 nanoparticles up to 16 wt% doubles the yield strength of nanocomposites. Tribological study showed that the friction coefficient was inversely related to WS 2 content. Probing the wear behavior of samples revealed more than 40% reduction in friction coefficient of nanocomposites compared to that of pure aluminum. Furthermore, the wear mechanism has changed from adhesive to adhesive-abrasive mechanism.
No takes yet. Share an insight, caveat, or question.
Vaziri et al. (2018) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: