The tissue/biomaterial interface reactions of four elastomers--selected as candidates for scaffolding for tympanic membrane tissue in a total alloplastic middle ear prosthesis--were studied at the electron microscopical level after implantation in the rat middle ear. Time-dependent changes in the phagocyte/polymer interface suggested degradation of porous implants made of Estane polyether urethane, polypropylene oxide, and a poly(ethylene oxide hydantoin) and poly(tetramethylene terephthalate) segmented polyether polyester copolymer (HPOE/PBT copolymer), but not of dense Silastic silicone rubber implants. Silastic was always encapsulated in fibrous tissue. Contact between fibrous tissue and HPOE/PBT copolymer or Estane was established in the third month, but fibrous tissue was never seen close to polypropylene oxide. Bone made contact only with Estane and HPOE/PBT copolymer implants. The bone/copolymer interface showed an electron-dense layer morphologically similar to that seen between bone and hydroxyapatite ceramic, suggesting that with respect to bone HPOE/PBT copolymer behaves like a bioactive implant material. The electron-dense layer was absnet at the bone/Estane interface. Estane and especially HPOE/PBT copolymer seem to be suitable as alloplastic tympanic membrane because of their interface behavior with respect to fibrous tissue and bone.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Bakker et al. (1990) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: