A magnetic sector secondary ion mass spectrometry (SIMS) instrument has been fitted with a modified hot filament duoplasmatron ion source for generation of SF5+ primary ion beams for SIMS depth profiling applications. The SF5+ primary ion beam has been evaluated by depth profiling of several low energy boron ion implants, boron delta-doped structures and a Ni/Cr metal multilayer depth profiling standard reference material. Using 3.0 keV impact SF5+ bombardment at a 52° impact angle with oxygen flooding gives a trailing edge decay length (1/e) for the boron implants and delta-doped layers of 1.3 nm. Under the same conditions, O2+ bombardment gives a trailing edge decay length (1/e) of 2.3 nm. The use of the SF5+ beam without oxygen flooding gives a substantial increase in decay length that is related to the formation of ripples as determined by atomic force microscopy. In the case of the Ni/Cr reference material, a significant reduction in sputter-induced topography is observed with SF5+ bombardment.
No takes yet. Share an insight, caveat, or question.
Gillen et al. (2000) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: