The formation of a solid electrolyte interphase (SEI)-type layer on films prepared by pulsed laser deposition on Pt coated p-doped silicon and cycled in 1 M in propylene carbonate is reported. The formation of the SEI was studied as a function of the voltammetric charging/discharging sweep rate at in the potential range of 3.5–4.4 V vs using high resolution scanning electron microscopy and energy-dispersive X-ray spectroscopy. By applying an asymmetric charging/discharging cycle, it is possible to enhance the SEI layer formation. The observed cycling dependence of the SEI is indicative of a continuous formation and degradation process of the SEI depending on the cycling direction and the sweep rate.