Poly(lactic acid) (PLA) is widely used in fused deposition modeling (FDM), but its recyclability is limited by cumulative thermomechanical degradation, and the combined effects of reprocessing, filler incorporation, and thermal aging on PLA/graphite composites remain poorly understood. This study addresses this gap by systematically investigating the effects of graphite content (0, 2.5, and 5.0 wt%), reprocessing cycles (1x, 5x, and 10x), and accelerated thermal aging at 105 °C on the structural, rheological, thermomechanical, and mechanical behavior of PLA-based composites for FDM. Reprocessing induced progressive matrix degradation, with melt flow rate increasing markedly and tensile strength decreasing by up to 35.6% for neat PLA after ten cycles. Graphite acted as a physical and microstructural modifier, improving stiffness and reducing moisture uptake under moderate reprocessing, but its reinforcing efficiency declined markedly under severe degradation. Accelerated thermal aging led to a rapid and substantial loss of tensile strength within the first days of exposure across all formulations, confirming the intrinsic thermal instability of the PLA ester backbone regardless of graphite content. These findings establish direct correlations between molecular-scale degradation and macroscopic performance, contributing to the rational design of recycled PLA/graphite filaments for circular economy-oriented FDM applications.
No takes yet. Share an insight, caveat, or question.
Dias et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: