Experimental study reveals increased sintering activation energy in cerium-doped yttria nanoparticles, indicating that grain boundary segregation impedes densification.
Cerium doped yttrium oxide nanoparticles with various Ce3+ concentrations between 0.001 and 0.010 at% have been synthesised by precipitation method using ammonium hydroxide as a precipitation agent. The synthesised powders are characterised by a mean particle size of ca. 55 nm. Highly dense specimens, with a relative density> 98.8%, were obtained by sintering the green compacts shaped by pressure filtration, at 1550 °C for 3 h in air. The sintering behaviour of Ce3+ doped Y2O3 was studied by constructing Master Sintering Curves (MSC); the results showed that the apparent activation energy of sintering for Ce3+ doped Y2O3 increases with the increase of cerium concentration. The segregation of larger Ce3+ cations in the grain boundaries is likely to be responsible for the increase in the sintering activation energy.
No takes yet. Share an insight, caveat, or question.
Govindan et al. (2022) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: