Data on the effect of various alkaline reagents on the physical and chemical properties of wool yarn are presented. When wool is treated with dilute sodiumhydroxide solutions, a rapid splitting off of a portion of the sulphur occurs. On continued treatment, the sulphur content of the residual wool approaches a constant value of about 1.8 percent. The results indicate that the alkaline treatment has changed a portion of the sulphur to a form which tends to resist further splitting from the molecule. Oxidizing and reducing agents attack the disulphide groups and make wool more susceptible to alkaline treatments. The susceptibility of untreated wool to alkaline reagents appears to be closely associated with the lability of its sulphur in alkaline solutions.