Answers are grounded in this paper and cite their sources.
The inhomogeneity of AA1060 aluminum and T2 copper friction welded joint was investigated through comparing the microstructure and properties at center, 1/2 R and edge positions along the radius. Sound joining was achieved at the center position of as-welded joint which fractured in the aluminum base metal, and the tensile strength decreased gradually from the center to the edge position, while the electrical resistivity increased. After heat-treated at 100 °C for 2 h, the joint had the highest integral tensile strength and the lowest electrical resistivity. When the joint was heat-treated at temperature above 400 °C, cracks formed in the interface and deteriorated the properties of joint. Part of intermetallic compounds layer in the center position of joint heat-treated at 400 °C disappeared. With increasing the heat treatment temperature or time, the disappearance of intermetallic compounds extended from the center to 1/2 R position. Al 4 Cu 9 phase grew faster than Al 2 Cu and AlCu phases. The growth rates of Al 2 Cu, AlCu and Al 4 Cu 9 phases were the fastest at the edge position and the slowest at the 1/2 R position. The activation energy of Al 2 Cu, AlCu, Al 4 Cu 9 phases and total intermetallic compounds were 92.24 kJ mol −1 , 55.59 kJ mol −1 , 146.92 kJ mol −1 and 121.40 kJ mol −1 , respectively.
No takes yet. Share an insight, caveat, or question.
Li et al. (2018) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: