Ti‐22Al‐25Nb joint was achieved by using linear friction welding (LFW) technique. The hot corrosion behavior of base metal, weld zone, and thermo‐mechanically affected zone (TMAZ) was investigated at 700 °C in 25% NaCl‐75% Na 2 SO 4 (wt%) mixed molten salt. In the initial stage, the base metal and joint exhibit similar oxidation resistant ability, and the corrosion products formed on all zones are mainly composed of TiO 2 , Nb 2 O 5 , and Al 2 O 3 . The formation of NaNbO 3 first occurs in base metal and TMAZ after 50 h, while the weld zone is free of NaNbO 3 until 100 h. The development of pitting corrosion in both base metal and TMAZ is caused by the diffusion of sulfur and re‐oxidation of sulfides. After a prolong exposure in molten salts, more serious sulfuration, acid dissolution, and escape of gaseous chlorides occurred in base metal leading to a drastic acceleration of corrosion rate.
No takes yet. Share an insight, caveat, or question.
Chen et al. (2018) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: