Answers are grounded in this paper and cite their sources.
Reactive ion etching of RbTiOPO4(0 0 1) substrates and (Yb,Nb):RbTiOPO4/RbTiOPO4(0 0 1) epitaxial layers has been performed using fluorine chemistry. A maximum etch rate of 8.7 nm/min was obtained, and the deepest etch achieved was 3.5 μm. The (Yb,Nb)-doped epitaxial layers showed a slower etching rate when compared with undoped material. Liquid phase epitaxial growth of cladding layers has also been performed, resulting in a high-quality interface growth without appreciable defects. 9-mm-long Mach-Zehnder interferometer and 9-mm-long Y-splitter structures were designed and patterned in RbTiOPO4substrates and (Yb,Nb):RbTiOPO4/RbTiOPO4(0 0 1) epitaxial layers. The structures fabricated in RbTiOPO4substrates were filled with laser active (Yb,Nb):RbTiOPO4higher refractive index core material, and finally an RbTiOPO4cladding was grown on the samples. The refractive index difference between the (Yb,Nb):RbTiOPO4layer and the RbTiOPO4substrate at 1.5 μm has been measured and optical waveguiding at this wavelength has been demonstrated.
No takes yet. Share an insight, caveat, or question.
Butt et al. (2014) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: