Answers are grounded in this paper and cite their sources.
Isothermal desorption of o-terphenyl thin-film bilayers was used to measure self-diffusion coefficients of supercooled o-terphenyl near the glass transition temperature (Tg=243 K). Diffusion coefficients from 10(-15.5) to 10(-12) cm2 s(-1) were obtained between 246 and 265 K. Protio and deuterio o-terphenyl were sequentially vapor deposited, then annealed to simultaneously diffuse and desorb the sample in a vacuum chamber. During the desorption of the bilayer, the concentration of each isotope was detected by a mass spectrometer, which revealed the extent of interfacial broadening. In these experiments, isotopic interdiffusion is indistinguishable from self-diffusion and the measured interfacial broadening is consistent with Fickian diffusion. The samples prepared under several different deposition conditions yielded the same self-diffusion coefficients, indicating that the experiments were conducted in the equilibrium supercooled liquid state.
No takes yet. Share an insight, caveat, or question.
Mapes et al. (2006) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: