Pure MgAl 2 O 4 and a series of Dysprosium (Dy 3+ ) doping in MgAl 2 O 4 nanoparticles has synthesized using wet chemical sol‐gel method and prepared samples were sintered at 1100 °C. X‐ray diffraction analysis confirms the cubic phase of MgAl 2 O 4 spinel without any impurity in phase even with different doping concentrations of Dy 3+ (0.2–1.8 mol %). Under ultraviolet irradiation (283 nm) the fluorescence spectrum of pure MgAl 2 O 4 shows maximum emission in the green‐yellow region. On Dy 3+ doping in MgAl 2 O 4 , broad emission spectra have been observed due to energy transition that takes place between the host and dopant. To explore the nanophosphor for white light, chromaticity coordinates (CIE), color temperature (CCT), color rendering index (CRI) and color purity were analyzed and at 1.4 mol % doping concentration of Dy 3+ in MgAl 2 O 4 got best results i. e. CIE co‐ordinates (0.3326, 0.3334), CCT (5487), CRI (95) and minimum value of color purity (0.20 %). It is observed that emission shifts from yellow‐green to nearly white light emission as the doping is incorporated into the host. It is found that the prepared nanophosphors are energy efficient white light material.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Kaur et al. (2023) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: