A postdeposition method of doping tin‐oxide films that includes ion implantation and a subsequent anneal has been developed. The method offers the advantage of being simpler and more reproducible than in situ doping techniques. Electrical conductivity can be controlled by adjusting dose and energy. Annealing at 700°C or above for 30 min is adequate to activate the dopants. Diffusion of the dopants such as phorphorus, arsenic, and fluorine in tin oxide is negligible at 900°C or below. Thus dopant distribution is essentially dependent on implant straggle. Electrical conductivity of 400 mho‐cm −1 can be routinely obtained with phosphorus implant. The highest conductivity achieved was 700 mho‐cm −1 with a combination of phosphorus and implants.