Answers are grounded in this paper and cite their sources.
A new double vacuum melting route (conventional second refining + vacuum arc refining [CSR + VAR]) with 33% lower production cost than the traditional VIM + VAR route has been tried. Compared with the CSR route, the CSR + VAR route reduces the average inclusion size from 27.1 ± 12.3 μm to 13.7 ± 2.4 μm, and the CSR + VAR steel processes a 13.1% higher rotatory bending fatigue (RBF) fatigue strength ( ) and a 3‐timeslonger RCF L 10 life. The crescent‐shaped granular bright facet (GBF) zone, normally found in high‐strength steels' very high cycle fatigue regimes beyond 10 7 cycles normally under a much lower stress amplitude, appears around inner inclusions on the CSR + VAR steel RBF fracture surfaces in high cycle fatigue regimes beyond 3 × 10 5 cycles. The development of GBF zones is estimated to account for 79%–90% of the RBF fatigue life. The average crack propagation rate (da/dN) for GBF zones varies from 1.3 × 10 −12 m/cycle to 24 × 10 −12 m/cycle and increases with the stress amplitude.
No takes yet. Share an insight, caveat, or question.
Shi et al. (2022) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: