Carrier mobility is one of the crucial parameters determining the electronic device performance. We apply the light-induced transient grating technique to measure independently the carrier diffusion coefficient and lifetime, and to reveal the impact of additives on carrier transport properties in wet-cast CH 3 NH 3 PbI 3 (MAPbI 3 ) perovskite films. We use the high excitation regime, where diffusion length of carriers is controlled purely by carrier diffusion and not by the lifetime. We demonstrate a four-fold increase in diffusion coefficient due to the reduction of localization center density by additives; however, the density dependence analysis shows the dominance of localization-limited diffusion regime. The presented approach allows us to estimate the limits of technological improvement—carrier diffusion coefficient in wet-cast layers can be expected to be enhanced by up to one order of magnitude.
No takes yet. Share an insight, caveat, or question.
Ščajev et al. (2018) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: