Answers are grounded in this paper and cite their sources.
A set of LiNi 0.5 Mn 0.3 Co 0.2 O 2 /graphite lithium-ion cells underwent 750 charge-discharge cycles during about 8 months at 55°C to upper cutoff potentials of 4.0, 4.1, 4.2, 4.3, and 4.4 V. The electrolyte in these cells was extracted using a centrifuge method and studied using gas chromatography/mass spectrometry to determine the changes to the solvents and by inductively coupled plasma-mass spectrometry to determine the changes to the salt content in the electrolyte. The negative electrodes from the cells were harvested and studied by micro-X-ray fluorescence to quantify the amount of transition metals which migrated from the positive electrode to the negative electrode during the testing. Emphasis is given to a detailed description of the quantitative methods used in the hope that others will adopt them in similar studies of different types of aged lithium-ion cells. The cells studied here initially had 1.1 molal LiPF 6 ethylene carbonate (EC): ethyl methyl carbonate (EMC) (3:7 by weight) electrolyte. The aged cells showed increasing amounts of dimethyl carbonate and diethyl carbonate created by transesterification as the upper cutoff potential increased. Only extremely small amounts of Mn, less than 0.1% of the total Mn in the positive electrode, were found on the negative electrode after this aggressive testing.
No takes yet. Share an insight, caveat, or question.
Thompson et al. (2018) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: