This is the authors' abstract. We don't add key points for this paper.
A dense α‐Si 3 N 4 ‐based ceramic protective coating was successfully prepared on porous Si 3 N 4 ceramics by a liquid infiltration and filling method. The coating composed of a primary α‐Si 3 N 4 phase and secondary O'‐Sialon, β‐Sialon, and Y–Si–Al–O–N glass phase. After thermal shock at Δ T = 1000°C for five times, cracks were produced, but the tip of crack stopped inside the coating; so the coated porous Si 3 N 4 ceramics still had a good waterproof ability and its water absorption was only 7%. During thermal shock, toughening mechanisms involving needle‐like O'‐Sialon particle bridging, crack deflection, and rough fracture, occurred within the cracks, contributing to thermal shock resistance of the coating. The dielectric constant of the coated porous Si 3 N 4 ceramics showed a slow increase trend with increasing temperature, and it reached the maximum value of 3.57 at 1100°C at the frequency of 11 GHz. The dielectric loss increased slowly as the temperature increased from room temperature to 900°C, but it started to increase evidently when the temperature was over 900°C.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Wang et al. (2019) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: