Answers are grounded in this paper and cite their sources.
Tin sulphide (Sn x S y ) thin films have been prepared on Pyrex glass substrates by the spray pyrolysis technique using tin chloride (SnCl 2 ) and n, n-dimethylthiourea (CH 3 NHCSNHCH 3 ) as starting materials. The depositions were carried out in the range of substrate temperatures from 320 to 450 degrees C. From X-ray diffraction measurements and SEM micrographs, it is found that the values of x and y, which determine the type of deposited compound, depend on the substrate temperature. At lower substrate temperatures (320-360 degrees C), mixed phases such as Sn 2 S 3 and gamma -Sn 2 S 3 are present. At intermediate substrate temperatures (370-390 degrees C), the SnS phase is predominant. For substrate temperatures higher than 390 degrees C the deposited material is mainly SnO 2 . The optical reflectance and transmittance of SnS were used in an iterative method to obtain the refractive index (n) and the extinction coefficient (k). These values of n and k were used to calculate the absorption coefficient ( alpha ) and the bandgap (E G ), giving the result E G =1.27 eV. Measurements of the dark conductance ( sigma ) as a function of T were made and an activation energy of 0.54 eV was determined from the slope of a plot of ln sigma versus 1/T.
No takes yet. Share an insight, caveat, or question.
López et al. (1994) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: