The intermediate layer (IL) between the glass and silicon plays an important role in laser-crystallized thin-film silicon solar cells. SiOX, SiNX, and SiCXdeposited by RF sputtering or plasma-enhanced chemical vapor deposition, either as single layers or in stacks, have been tested as ILs with regard to silicon wettability and silicon crystal quality and the effect of hydrogen passivation. SiCXis the best wetting layer, allowing a larger laser crystallization process window than SiOXor SiNX. SiNXlayers are limited by pinholing, which increases in severity with laser fluence. SiOXILs result in lower silicon grain-boundary density compared with SiCx-based layers and to SiNX-based layers. Hydrogen passivation of laser-crystallized silicon on single layer SiOXhas no impact on VOC, while an improvement of around 60 mV is found for samples on SiOx/SiNx/SiOxstacks. Diffusion of dopants from the IL are found to create a uniformly doped absorber with no evidence of a front-surface field.
No takes yet. Share an insight, caveat, or question.
Dore et al. (2014) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: