Answers are grounded in this paper and cite their sources.
The thermoelectric power Θ and the electric resistance R of soft and hard carbons were investigated as functions of heat-treatment temperature Tₕₜ from 1000^∘{}C to 3100^∘{}C at three ambient temperatures T equal to 90^∘{}K, 305^∘{}K, and 573^∘{}K. The crystalline structure was studied by means of x-ray powder diffraction technique. For a given T, with increase of Tₕₜ the thermoelectric power of soft carbons goes through a flat minumum at Tₕₜ~1400^∘C, increases quite fast to a maximum at about 2100^∘{}C, and subsequently drops down again and continues to do so up to the highest Tₕₜ. The electric resistance is only very slowly decreasing (plateau) up to Tₕₜ~2000^∘C, with a subsequent rapid decrease up to the highest Tₕₜ investigated. The positions of the maximum in Θ and of the corresponding knee in resistance (end of plateau) shifts to higher heat treatments with decrease of ambient temperature T. The thermoelectric power is proportional to temperature T in the range of heat treatments below the Tₕₜ corresponding to the maximum in Θ. The observed dependence of Θ and of R on Tₕₜ and T are in good agreement with Mrozowski's energy band scheme for carbons and graphites. A hard carbon prepared from phenol-benzaldehyde resin shows a two-stage graphitization with 1/8 of the crystalline mass beginning to graphitize at Tₕₜ~2200^∘C and the remainder only above Tₕₜ=2800^∘C. Correspondingly the resistance curves show two plateaus ending one at Tₕₜ~2200^∘C and the other at Tₕₜ~2800^∘C. The dependence of Θ on Tₕₜ is somewhat similar to that found in soft carbons.
No takes yet. Share an insight, caveat, or question.
E. E. Loebner (1956) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: