The new nitridoalumosilicate phosphor SrAlSi 4 N 7:Eu 2+ has been synthesized under nitrogen atmosphere at temperatures up to 1630 °C in a radio-frequency furnace starting from Sr metal, α-Si 3 N 4, AlN, and additional Eu metal. The crystal structure of the host compound SrAlSi 4 N 7 has been solved and refined on the basis of single-crystal and powder X-ray diffraction data. In the solid, there is a network structure of corner-sharing SiN 4 tetrahedra incorporating infinite chains of all edge-sharing AlN 4 tetrahedra running along [001] (SrAlSi 4 N 7: Pna 2 1 (No. 33), Z = 8, a = 11.742(2) Å, b = 21.391(4) Å, c = 4.966(1) Å, V = 12.472(4) Å 3, 2739 reflections, 236 refined parameters, R 1 = 0.0366). The Eu 2+ -doped compound SrAlSi 4 N 7:Eu 2+ shows typical broadband emission originating from dipole-allowed 4f 6 ( 7 F J )5d 1 → 4f 7 ( 8 S 7/2 ) transitions in the orange-red spectral region (λ max = 632 nm for 2% Eu doping level, 450 nm excitation) with a spectral width of FWHM = 2955 (± 75) cm −1 and a Stokes shift Δ S = 4823 (± 100) cm −1 . The luminescence properties make the phosphor an attractive candidate material as red component in trichromatic warm white light LEDs with excellent color rendition properties.
No takes yet. Share an insight, caveat, or question.
Hecht et al. (2009) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: