NaxCu9S5 (x = 0, 0.025, 0.05, 0.15, 0.25) nanopowders with an average size of 3 nm are prepared by ball milling and are then sintered with spark plasma. Due to the small size of the nanopowders, the bulk materials possess very fine grains after sintering. The highest ZT value is about 1.1 at 773 K and is obtained for Na0.05Cu9S5 sample that is nearly threefold higher than that of pristine Cu9S5 and comparable to the modified PbS materials (ZT ≈ 1.2 at 923 K).