Nonstoichiometric LiNi 0.5 Mn 1.5 O 4 - δ and stoichiometric LiNi 0.5 Mn 1.5 O 4 cathodes with two different structures ( Fd 3̄ m and P 4 3 32) were synthesized by a molten salt method. Rietveld refinement of the X-ray diffraction (XRD) data and a selected-area electron diffraction (SAED) study confirmed that the face-centered spinel ( Fd 3̄ m ) transformed to the primitive simple cubic ( P 4 3 32) upon additional heating at 700 °C. The LiNi 0.5 Mn 1.5 O 4 - δ cathode having the space group of Fd 3̄ m showed better electrochemical behaviors than did the LiNi 0.5 Mn 1.5 O 4 cathode with the space group of P 4 3 32, specifically, a lower area-specific impedance (ASI) and a higher discharge capacity during cycling at high rate. XRD and SAED showed that both stoichiometric and nonstoichiometric LiNi 0.5 Mn 1.5 O 4 - δ exhibited similar SAED patterns with extra 002 spots at the fully delithiated state, suggesting a structural transition arising from the possible migration of transition metal cations during Li extraction. In addition, stoichiometric LiNi 0.5 Mn 1.5 O 4 ( P 4 3 32) had an intermediate phase of Fd 3̄ m during Li extraction. Such a two-step phase transition of stoichiometric LiNi 0.5 Mn 1.5 O 4 ( P 4 3 32) induced low structural reversibility at a high rate (3C rate). Meanwhile, nonstoichiometric LiNi 0.5 Mn 1.5 O 4 - δ ( Fd 3̄ m ) exhibited good structural reversibility, as confirmed by XRD and SAED for the cycled electrode even at high rate (3C rate).
No takes yet. Share an insight, caveat, or question.
Kim et al. (2004) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: