In this paper, the point-defect interactions which occur during annealing, when doping diamond by means of the cold-implantation--rapid-annealing technique [Phys. Rev. B 38, 5576 (1988)], are modeled using reaction-rate theory. The equations predict that the magnitudes of the activation energies, controlling dopant--interstitial-vacancy combination and dopant-interstitial diffusion, relative to the same energies applicable to the self-interstitials, determine the end result which will be obtained for a chosen implantation-annealing sequence. It is also possible to explain why an increase in the annealing temperature can lead to a decrease in dopant activation, as had been observed experimentally (and reported elsewhere) for boron. Reasonable values for the self-interstitial activation energies are found when applying this model to previously published results.
No takes yet. Share an insight, caveat, or question.
Johan F. Prins (1991) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: