Demonstrates that the power-to-pressure ratio in PECVD characterizes silicon-surface passivation, indicating an optimal processing window for heterojunction solar cells.
The hydrogen content ( C H ) and microstructure of a hydrogenated amorphous-silicon (a-Si:H) layer fabricated by plasma-enhanced chemical vapor deposition (PECVD) were analyzed to determine the effect of surface passivation on crystalline silicon (c-Si). The ratio of radio-frequency power to gas pressure ( C pp in W·Pa −1 ) of the PECVD system is defined as a characterization parameter. It was found that C H and the passivation of a-Si:H layers were sensitively affected by C pp . However, C H remained almost constant at the same C pp even though the PECVD power and pressure were widely varied. We determined that an optimal region exists in the range of 0.75 < C pp < 1.25, where a high implied open-circuit voltage of 732 mV was obtained from a passivated a-Si:H/c-Si/a-Si:H structure, indicating that C pp was a useful parameter for characterizing the surface passivation effect of a a-Si:H layer on c-Si.
No takes yet. Share an insight, caveat, or question.
Guo et al. (2015) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: