Answers are grounded in this paper and cite their sources.
Polyurethanes were prepared from polycaprolactone, 4, 4′-diphenylmethane diisocyanate, and ethylene diamine. Two kinds of polymers were used for the present experiments. One contained polycaprolactone with the number-average molecular weight, , of 1.30×103, while the other contained polycaprolactone with an value of 2.80×103. Each polymer was fractionated from a dimethyl acetamide solution by progressive precipitation with a mixture of n-heptane and ethyl ether, and the fractions were characterized in terms of viscosity and sedimentation. The relations between the intrinsic viscosity and the molecular weight were found in DMF at 25°C to be: [η]=5.52×10−4M0.66 for the polymer containing polycaprolactone (=1.30×103) and [η]=7.71×10−4M0.62 for the polymer containing polycaprolactone (=2.80×103). The viscosities of the solutions of the polymers were measured in several solvents at different temperatures, and the polymer-solvent interaction parameters were obtained by using the Fixman theory for the expansion factor. The molecular-weight distribution of the polymer containing polycaprolactone (=1.30×103) was obtained from the distribution of the sedimentation coefficient, while the value of ⁄ was calculated from the distribution curve to be 1.95.
No takes yet. Share an insight, caveat, or question.
Hiroshi Satō (1966) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: