Answers are grounded in this paper and cite their sources.
Explores defect dynamics in thin films, suggesting implications for coating performance.
This study explores the evolution and distribution of open-volume defects in magnetron-sputtered Al (60 and 100 nm), Fe 3 O 4 (120 nm), and Al–Fe 3 O 4 (220 nm) composite thin films through a synergistic experimental and theoretical approach. Doppler Broadening Positron Annihilation Spectroscopy (DB-PAS) was utilized to profile the S and W parameters across varying implantation energies, enabling a depth-resolved characterization of the structural defects. While individual Al and Fe 3 O 4 films exhibited characteristic linear-type defects, the Al – Fe 3 O 4 composite demonstrated a distinct shift toward vacancy-type defect dynamics. Theoretical MIKA/ATSUP calculations were used to evaluate representative Fe-vacancy and Fe-O-vacancy positron-annihilation fingerprints, while EMD/DECOMP analysis related the Doppler features to the Fe-O electronic structure. The results indicate a Fe 3 O 4 -like, rather than metallic-Al-like, annihilation response and support defect-related electron-density redistribution at the Al/Fe 3 O 4 interface, without assigning a unique microscopic defect. Electron Momentum Distribution (EMD) analysis further confirmed that the contact between Al and Fe 3 O 4 layers induces interface-driven defect passivation and electronic hybridization, where Al valence electrons effectively screen the open-volume defects in the oxide matrix. These insights into the interplay between interfacial interactions and defect stabilization suggest that the Al– Fe 3 O 4 system achieves superior structural compactness, positioning it as a promising candidate for high-performance, corrosion-resistant coatings in nanostructured functional materials.
No takes yet. Share an insight, caveat, or question.
Ahmadova et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: