Answers are grounded in this paper and cite their sources.
Highly selective etching of with respect to silicon and resist is obtained by reactive ion etching in . The maximum etch rate ratio depends in a sensitive way on gas residence time with etch rate ratio increasing with decreasing residence time. The reproducibility of high etch rate ratios was found to decrease with increasing pressure. The cleanliness of etching is determined by the material of the electrode and the electrode to wall area ratio. A process was developed by optimizing etching conditions and reactor design and then was tested electrically. Contact holes were etched to 0.25 μm junctions using full RIE in and buffered . The same low junction leakage and contact resistivity, 10 −9 amps/cm 2 and 10 −6 Ω‐cm 2 , were measured for both. Implications for scaling RIE into larger etching reactors as well as its use to pattern features at 1 μm ground rules are discussed.
No takes yet. Share an insight, caveat, or question.
Ephrath et al. (1982) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: