Elastomeric polyurethane (PU) was mixed with 1, 3, 5, 7, and 10 wt% of Cloisite 20A to obtain PU-based nanocomposites. The thermal stabilities of the obtained products were characterized by thermal analysis using a thermogravimetric analyzer (TGA), which showed that addition of 5 wt% of organoclay to the PU increased its stability, whereas thermal stabilization was less efficient at 10 wt%. The electrical conductivities of these composites were studied as a function of temperature, and it was found that the conductivity of PU was enhanced upon using 5 wt% of organoclay. The tensile strength, elongation (%), and Young's modulus were considerably enhanced upon increasing the organoclay content to 5 wt%, but were then decreased to some extent upon further increase of the nanoparticle loading to 10 wt%. X-ray diffraction (XRD) and scanning electron microscopy (SEM) were used to study these nanocomposite structures, and it was found that the organoclay is fully exfoliated in the PU matrix when 5 wt% of Cloisite 20A was used.
No takes yet. Share an insight, caveat, or question.
Dimitry et al. (2011) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: