Solution and diffusion of He, Ne, Ar, Kr, Xe, H 2 , N 2 , O 2 , and n ‐C 4 H 10 have been studied in filled dimethylpolysiloxane elastomers, at temperatures between 0 and −37°C. for all penetrants, and down to −78°C. for some. Crystallization of the rubber, commencing at about −50°C. resulted in large decreases in permeability and diffusion coefficients and smaller decreases in solubility. Diffusion coefficients were measured in three different ways and solubility coefficients in two. Above the crystallization temperature, the results by all methods agreed for a lightly filled rubber but for a rubber with a high filler content especially when partially crystalline (i.e., below −50°C.) differences were observed between solubility coefficients measured directly and those derived from permeation and diffusion. These differences arc related to the heterogeneity of the medium and to consequent differences in diffusion coefficients obtained by the time‐lag and steady‐state methods. Diffusion and solubility coefficients both show relationships with other physical properties. Permeabilities of the silicone rubbers to gases are high, and selectivity can be good as between appropriate pairs of molecules.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Barrer et al. (1965) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: