Answers are grounded in this paper and cite their sources.
When processing powder metallurgy (PM) steels, the conventional press and sinter route can reach a relative density up to 95%, which is insufficient for applications when dynamic mechanical performance is critical. In this study, a novel route is demonstrated consisting of cold isostatic pressing (CIP) followed by sintering and capsule-free hot isostatic pressing (HIP), allowing to achieve full density PM steels. Water-atomized steel powder admixed with 2 wt.% Ni was subjected to CIP and followed by sintering in 90N 2 /10H 2 atmosphere at 1120 and 1250°C, and in vacuum (10 −2 mbar) at 1250 and 1350°C, respectively. At the highest explored CIP pressure of 600 MPa, the three high-temperature sintering runs at 1250°C in 90N 2 /10H 2 atmosphere and vacuum, and 1350°C in vacuum resulted in relative density of ∼94% and closed surface pores. This condition with necessary closed porosity then allowed subsequent capsule-free HIP after sintering, resulting in full densification of the components.
No takes yet. Share an insight, caveat, or question.
Nagaram et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: