Pr 1.0− x Gd x Co 5.7 CuTi 0.3 ( x = 0.0–0.5) samples have been prepared by arc melting and precipitation hardening. X-ray diffraction and transmission electron microscopy reveal that their microstructures consist of a rhombohedral 2 : 17 matrix phase surrounded by a hexagonal 1 : 5 cell boundary phase. Gd addition leads to an increase in the Curie temperatures of both the 1 : 5 and 2 : 17 phases. The temperature coefficient of saturation magnetization (η = d J s /d T ) increases with increasing x and a nearly zero η is obtained in the magnet with x = 0.5. Positive temperature coefficients of coercivity H c and energy product ( BH ) max have been observed in all samples. Thus, H c of about 0.7 T and ( BH ) max of about 3.0 MG Oe are obtained in the Gd-substituted sample at high temperatures. The magnetization reversal of the Pr–Co based precipitation-hardened magnets is dominated by domain-wall pinning in the whole temperature range.
No takes yet. Share an insight, caveat, or question.
Rong et al. (2004) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: