Answers are grounded in this paper and cite their sources.
The H 2 O layer thickness on flat hydroxylated SiO 2 surfaces was measured at various H 2 O pressures and substrate temperatures using in situ real-time spectroscopic ellipsometry (SE). The in situ SE measurements were conducted at 18.1, 27.2, and 30.4 °C (291.25, 300.35, and 303.55 K) in a warm-wall vacuum chamber designed with a cooled sample stage. The H 2 O pressures were varied up to the saturation H 2 O vapor pressures of 15.6, 27.0, and 32.5 Torr at 18.1, 27.2, and 30.4 °C, respectively. The SE measurements showed that there were two distinct types of H 2 O layers on the hydroxylated SiO 2 surface: a thin strongly adsorbed layer and a weakly adsorbed layer that was much thicker at high H 2 O pressures. The strongly adsorbed layer had thicknesses ≤1.2 Å and was not lost by removing the H 2 O pressure. The strongly adsorbed layer could be desorbed by heating the sample stage to 124 °C (397.15 K). The stability of the strongly adsorbed layer was consistent with an adsorption energy of >20 kcal/mol. In contrast, the weakly adsorbed layer could be added or removed by increasing or decreasing the H 2 O pressure. The weakly adsorbed layer obtained much higher multilayer H 2 O thicknesses at larger H 2 O pressures. For example, the weakly adsorbed multilayer thickness was 7.5 Å at 92% relative humidity at 30.4 °C (32.5 Torr). Complementary in situ Fourier transform infrared (FTIR) studies were also performed on hydroxylated SiO 2 nanoparticles that were in qualitative agreement with the SE results.
No takes yet. Share an insight, caveat, or question.
Râu et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: