This is the authors' abstract. We don't add key points for this paper.
A new semi-quantitative method was developed to detect Li deposition on Si/graphite anodes. This method is based on Post-Mortem glow discharge optical emission spectroscopy (GD-OES) depth profiling. Based on the contents of Si, Li, and O in the GD-OES depth profiles, we define a corridor, in which the minimum amount of metallic Li on the anode is located. This method was applied to three types of commercial 18650 cells with Si/graphite anodes in the fresh state and with Li plating intentionally produced by cycling at low temperatures. Additional cells were cycling aged at 45 °C to 80% SOH. The main aging mechanisms at 45 °C were determined using differential voltage analysis (DVA), SEM, and half cell experiments. Subsequently, the cells aged at 45 °C were further cycled under the conditions that had led to Li deposition for the fresh cells. Furthermore, the anode coating thickness for 18 types of commercial Li-ion cells are correlated with the specific energy, while distinguishing between graphite anodes and Si/graphite anodes. Our extensive Post-Mortem study gives deep insights into the aging behavior of state-of-the-art Li-ion cells with Si/graphite anodes.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Richter et al. (2022) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: