A scCO 2 drying/lixiviation process allows self-standing inorganic macrocelullar aerogels to be produced within 1 h. The applied depressurization rate permits the macrocellular internal throats to be tuned with native hydrodynamic instability. scCO 2 treatment advantageously addresses lixiviation of the tensioactive molecules employed as the templating agent. Final calcined aero-Si(HIPE) materials, at the optimum temperature of 450 °C, afford a specific surface area of up to 1400 m 2 g –1 . The lower treatment temperature and lower tension-active contents dramatically reduce the carbon footprint penalty, compared with that of traditional xero-Si(HIPE). Further annealing of these aero-Si(HIPE) foams at 1200 °C drastically decreases the specific surface area while maintaining both the open macroposity and the self-standing character. Concomitantly, severe shrinkage and densification of the monoliths occur upon cristobalite crystallization. For the sake of making this generic endeavor, the scCO 2 drying/lixiviation approach has also been extended to MUB-110, MUB-200, and MUB-300 co-oxide(HIPE) catalysts describing the same scenario of fostering the specific surface area, maintaining the monolith-type character and associated macroporous open tortuosity, and minimizing the carbon footprint penalty.
No takes yet. Share an insight, caveat, or question.
Layan et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: