Electrical resistivities in the range 1.1 to 35^∘{}K and magneto-resistivities in the range 1.1 to 4.2^∘{}K have been measured in a number of dilute, superconducting hcp Ti alloys. Resistivity minima occurring between 14 and 18^∘{}K are observed in {≈}99.92% pure Ti, and in Ti-Mn alloys with Mn concentrations between 0.02 and 2.0 at.% (nominal atomic percent). Negative magneto-resistivities between 2.6 and 7.2% at 30 kG and 4.2^∘{}K are observed in Ti-Mn alloys with Mn concentrations between 0.1 and 2.0 at.%. The absolute magnitude of the negative magnetoresistance increases as temperature decreases for Tₛ<T<4.2^∘K, where Tₛ is the temperature at which the zero-field resistivity begins to decrease due to the onset of supercouductivity. Field- and temperature-dependent Hall coefficients are observed at liquid helium temperatures in Ti containing Mn concentrations of 1.0 and 2.0 at.%. Ti alloys containing 1.2 at.% Cr and 0.96 at.% Fe display resistivity minima at about 17^∘{}K, but, unlike Ti-Mn alloys, they have small positive magnetoresistivities and do not exhibit field-dependent Hall coefficients at 4.2^∘{}K. Neither negative magneto-resistivities nor significant resistivity minima are observed in Ti containing 1.3 at.% Co, 1.0 at.% Ni, 1.1 at.% Al, or 1.0 at.% Nb. Considered in the light of recent ideas regarding the origin of the low-temperature resistive anomalies, the data suggest that localized magnetic moments exist in dilute superconducting Ti alloys containing Cr, Mn, and Fe, and that the conduction electrons interact with these moments.
No takes yet. Share an insight, caveat, or question.
Hake et al. (1962) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: