X-ray diffractometer traces obtained from PVC samples maintained at temperatures in the range 180 to 200°C indicate that crystal melting is followed by a state of intermediate order rather than by a truly amorphous state. In addition, this study raises serious doubts regarding the validity of the assumption that the x-ray scattering profile from quenched PVC samples is representative of the amorphous phase. Any crystallinity values derived on the basis of that assumption are therefore open to question.
No takes yet. Share an insight, caveat, or question.
Guerrero et al. (1981) studied this question.