In vitro study reveals insufficient curing depth in bulk-fill resin-based composites at 4 mm, indicating potential risks of placing large single increments in dental restorations.
This study evaluated the depth of cure (DOC) of packable and flowable bulk-fill resin-based composites (RBCs) including PRG (prereacted glass ionomer) and short-fiber materials. The materials were placed in a black split-mold with a 7 mm deep recess and cured at 700 mW/cm(2) for 20 s using a LED curing light. DOC was assessed using the ISO scraping and Knoops hardness tests. Data (n=5) were computed and analyzed using one-way ANOVA/Scheffe's post hoc test (p<0.05). ISO DOC ranged from 3.66 to 2.54 mm while DOC based on hardness testing ranged from 3 to 1.5 mm. For all materials, a decrease in hardness was observed with increasing depths. The DOC of bulk-fill RBCs was product dependent and greater than standard composites. At 4 mm depth, none of the bulk-fill RBCs had a depth: top hardness ratio of 0.8 and above.
No takes yet. Share an insight, caveat, or question.
Yap et al. (2016) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: