The present study assessed the polymerization shrinkage stress kinetics of five low-shrinkage light-cured bulk-fill resin composites: Surefil SDR flow (SF, Dentsply), Tetric EvoCeram Bulkfil (TE, Ivoclar Vivadent), Venus Bulk Fill (VB, Heraeus Kulzer), x-tra fil (XF, Voco), and experimental bulk fill (FB, 3M ESPE). Filtek Z250 (FZ, 3M ESPE) was used as a control. Real-time shrinkage stress of investigated composites was measured using a tensometer; maximum shrinkage stress, stress rate (Rmax), and time to reach maximum stress rate (tmax) were recorded. Flexural strength and modulus were measured using a standard procedure, and curing efficiency of 4-mm long specimens was determined using bottom/top percentage Knoop microhardness. Data were analyzed using one-way analysis of variance and Bonferroni multiple range tests at a significance level of α=0.05. Results of shrinkage stress, Rmax, and tmax of all bulk-fill materials were significantly lower (p<0.05) than those of the control except for XF. All tested bulk-fill materials were able to achieve acceptable curing efficiency (≥80% bottom/top percentage) at 4-mm depth. In conclusion, this study reports a significant reduction in polymerization shrinkage stress while maintaining comparable curing efficiency at 4 mm for some bulk-fill composites and supports their potential use in posterior clinical situations.
No takes yet. Share an insight, caveat, or question.
El‐Damanhoury et al. (2013) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: