Answers are grounded in this paper and cite their sources.
A TC17 titanium (Ti) alloy, with and without surface nanocrystallization (SN) treatment was joined to another Ti alloy, TC4, via solid-state diffusion bonding. The interfacial void shrinkage of SN-TC17/TC4 bond was accelerated comparing with that of coarse-grained TC17/TC4 bond. Dynamic recovery and recrystallization were mainly responsible for the fiber texture in β phase and the random orientation in α phase on SN-TC17 side, respectively. The promoted grain growth effect on SN-TC17 side at 1093 K contributed to the disappearance of original bond line (BL). The shear strength of SN-TC17/TC4 bond increased as bonding temperature increased to 1013 K due to the enhanced void shrinkage process, which further increased up to 789 MPa at 1093 K as a result of the disappearance of original BL. Moreover, the shear strength of SN-TC17/TC4 bond at 1093 K was about 60 MPa higher than that of TC17/TC4 bond due to the disappearance of original BL and the Hall–Petch strengthening effect.
No takes yet. Share an insight, caveat, or question.
Li et al. (2022) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: