CeF 3, CeF 3:Tb 3+, and CeF 3:Tb 3+ /LaF 3 (core/shell) nanoparticles were prepared by the polyol method and characterized by X-ray diffraction (XRD), transmission electron microscopy (TEM), X-ray photoelectron spectra (XPS), UV−vis absorption spectra, photoluminescence (PL) spectra, and lifetimes. The results of XRD indicate that the obtained CeF 3, CeF 3:Tb 3+, and CeF 3:Tb 3+ /LaF 3 (core/shell) nanoparticles crystallized well at 200 °C in diethylene glycol (DEG) with a hexagonal structure. The TEM images illustrate that the CeF 3 and CeF 3:Tb 3+ nanoparticles are spherical with a mean diameter of 7 nm. The growth of the LaF 3 shell around the CeF 3:Tb 3+ core nanoparticles resulted in an increase of the average size (11 nm) of the nanopaticles as well as in a broadening of their size distribution. These nanocrystals can be well-dispersed in ethanol to form clear colloidal solutions. The colloidal solutions of CeF 3 and CeF 3:Tb 3+ show the characteristic emission of Ce 3+ 5d−4f (320 nm) and Tb 3+ 5 D 4 − 7 F J ( J = 6−3, with 5 D 4 − 7 F 5 green emission at 542 nm as the strongest one) transitions, respectively. The emission intensity and lifetime of the CeF 3:Tb 3+ /LaF 3 (core/shell) nanoparticles increased with respect to those of CeF 3:Tb 3+ core particles. This indicates that a significant amount of nonradiative centers existing on the surface of CeF 3:Tb 3+ nanoparticles can be eliminated by the shielding effect of LaF 3 shells. Finally, the energy transfer from Ce 3+ to Tb 3+ was investigated in CeF 3:Tb 3+ nanoparticles in detail.
No takes yet. Share an insight, caveat, or question.
Wang et al. (2006) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: