The thermal oxidation of (100) and (110) GaAs at temperatures of 450-760 degrees C has been studied using Rutherford back-scattering. The oxide thickness formed on (110) GaAs increases with time according to a parabolic law provided the law thickness is less than about 1000 AA. Thicker oxides appear to grow at an increased rate (linear growth) compared with that expected from a parabolic law. Growth for 1 1 / 2 h on (110) GaAs produced a maximum thickness between 550 and 600 degrees C and a minimum near 650 degrees C. Above about 650 degrees C the growth rate increased with increasing temperature. The oxidation rate on (100) orientations was much less than that on (110) surfaces between 550 and 700 degrees C.