A titanium-niobium-wollastonite (Ti-Nb-CaSiO 3 ) composite was developed using mechanical alloying and powder metallurgy methods. The composite was then pressed conventionally and sintered at three different temperatures (800 °C, 1000 °C, and 1200 °C) under an argon gas environment. With the rise in temperature to 1200 °C, there was an observed increase in both the compressive strength (248.52 MPa) and elastic modulus (58.90 GPa). This can be attributed to the improved densification (5.263 g/cm 3 ) and decrease in porosity (9.33%). Upon immersion in Hank’s Balanced Salt Solution (HBSS) for 30 days, apatite deposition corresponding to Ca, P and O layers forms on the surface of the composite. At 1200 °C, the Ti-Nb-CaSiO 3 composite demonstrated increased apatite coverage due to ion leaching from the composite surface, resulting in an amorphous structure, indicating its potential for faster bone regeneration. Based on the results, the produced Ti-Nb-CaSiO 3 composite is a viable material for load-bearing orthopaedic applications, offering a balanced combination of mechanical integrity and bioactivity evaluation.
No takes yet. Share an insight, caveat, or question.
Zuhailawati Hussain (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: