Answers are grounded in this paper and cite their sources.
A nanometric Mg(OH)2 and MgO particles with high purity were successfully synthesized from Algerian dolomite via a leaching-precipitation-calcination process. The effect of leaching parameters, such as H2SO4 acid concentration (C), temperature (T), time (t), solid/liquid ratio (S/L), and precipitation parameters: type of precipitating base (KOH, NaOH, NH4OH), OH-/Mg2+ ratio, and temperature on the obtained product properties, were investigated using Taguchi approach. The optimal leaching conditions were selected as: C=5M, T=65?C, t=15 min, and S/L ratio=1:5. Furthermore, the potassium hydroxide (KOH) was selected as the optimal precipitating base with OH-/Mg2+ = 10.5. The calcination of the precipitates at 800?C during 2 h made it possible to produce a high purity MgO (~99.45 %) with a crystallite size of approximately 16.5 nm and particles in the form of agglomerated porous plates with a high SSA (70.42 m2/g) which may be of interest for some applications, such as catalysts or supports.
No takes yet. Share an insight, caveat, or question.
Bouchekrit et al. (2023) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: