This is the authors' abstract. We don't add key points for this paper.
As a sequel to our previous report on the key concept of the multiwidth (MW) no-insulation (NI) winding technique that applies the NI technique to a magnet assembly of double-pancake (DP) coils wound with varying tape widths (thus MW), this paper presents construction and test results of a 7-T/68-mm cold-bore MW-NI GdBCO magnet. A total of 13 DP coils were fabricated: five central DP coils were wound with 4.1-mm wide tape, while each of the remaining four pairs of DP coils, axially symmetric to the midplane, was wound, from center to end, with 5.1-, 6.1-, 7.1-, and 8.1-mm wide tapes. Each DP coil was tested in a bath of liquid nitrogen (LN2) at 77 K, to obtain its critical current and characteristic resistance. After stacking, the 13-DP magnet was tested in LN2 at 77 K. The key focuses of this paper are: 1) winding and testing of MW-NI DP coils; 2) DP–DP joints; 3) charging response of the magnet; 4) spatial field distribution; and 5) self-protecting feature in overcurrent operation.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Hahn et al. (2014) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: