The objective of this study was to determine the effect of surface Cr content on the corrosion of ferritic stainless steels in hot-pressurized alkaline water (310°C at 10 MPa) simulating a hydrothermal liquefaction bioconversion medium. Two methods to increase the Cr surface content were investigated: (i) selecting commercial grades of ferritic stainless steel with an increasing Cr content and (ii) applying a Cr coating (chromizing) to a low-Cr (Type 409) ferritic stainless steel. The observed parabolic-like corrosion kinetics were analyzed and discussed in terms of the structure and composition of the double-layered oxide films that formed. The (surface) Cr content is a critical factor affecting corrosion. Corrosion was reduced by 66% (after 20 d exposure) when increasing the Cr content from 9 wt% (P91) to 21 wt% (SS443) in the commercial grades of ferritic stainless steel. Moreover, corrosion was reduced by 84% (after 20 d exposure) by chromizing the surface of a low-Cr (Type 409) ferritic stainless steel. Improved corrosion protection was attributed to increased Cr incorporation into the inner (barrier) Fe(Fe1-nCrn)2O4 layer, with the formation of a Cr2O3 layer (resulting from chromizing) being most beneficial.
No takes yet. Share an insight, caveat, or question.
ASARE et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: