This study aimed to evaluate how DBD plasma treatment parameters influence the molecular structure and functional performance of gelatin powder. Gelatin samples were treated using DBD plasma at 16, and 18 kV for 0, 5, 10, and 15 min, and the resulting changes were evaluated through molecular, physicochemical, and functional analyses. SDS-PAGE results showed a distinct band formation around 60 kDa under severe plasma conditions, indicating polypeptide fragmentation. Free sulfhydryl increased 5 times at 16 kV for 10 min compared to control sample, followed by a marked reduction at higher plasma intensity, confirming oxidation-driven disulfide bond formation. FT-IR spectroscopy demonstrated measurable shifts in the amide I region, accompanied by an increased proportion of random coil structures. Plasma treatment reduced the zeta-potential of gelatin dispersions from ∼ -24 to ∼ -21 mV, reflecting alterations in surface charge distribution. Rheological measurements showed higher storage modulus and elastic behavior under moderate plasma conditions, whereas prolonged or high-voltage treatment resulted in weakened gel structures. Microstructure revealed smaller and uniform pores at mild plasma intensity and enlarged, irregular pores under sever conditions. The results demonstrate that DBD plasma induces quantifiable molecular and structural changes in gelatin, which can be strategically controlled to tailor its functional properties.
No takes yet. Share an insight, caveat, or question.
Anari et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: